MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sika Level-225 Superior flow, cementitious, self-leveling underlayment
Categories: Ceramic; Concrete

Material Notes: Sika® Level-225 is a one-component, durable and versatile cementitious underlayment for interior concrete and cementitious substrates. It can be applied manually or by pump to produce a self-smoothing, rapid-setting, flat and economical substrate prior to the application of a final floor finish. Typical application thickness is 1/16” – 1.25” (1.5 - 31 mm), or up to 2.5” (65 mm) with aggregate.

Where to Use: Interior floor leveling and smoothing applications where floor coverings are to follow, such as:
Institutional - schools, colleges, hospitals, clinics, libraries, galleries, museums
Commercial - stores, offices, corridors, hallways, cafeterias, hotels, restaurants
Residential - domestic properties, condominiums and high rise construction

Advantages:

  • Superior workability for easy installations
  • Very smooth surface
  • Fast dry time
  • Zero VOC content and low odor
  • Highly fluid self-leveling
  • Manual or pumpable application
  • Levels new and renovates old floors
  • Excellent underlay for tiles, sheet products and wood floor bonding systems

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.08 g/cc
Volatile Organic Compounds (VOC) Content 0.00 g/lEPA method 24
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 1250 psi
@Time 2.42e+6 sec
ASTM C348
Compressive Strength 1500 psi
@Time 86400 sec
ASTM C109
 3000 psi
@Time 605000 sec
ASTM C109
 4500 psi
@Time 2.42e+6 sec
ASTM C109
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hourReady for Foot Traffic
 3.00 hourReady for Tiles or Stone
 16.0 hourReady for Floor Covering
 45.0 - 65.0 minInitial set; ASTM C191
 65.0 - 75.0 minFinal set; ASTM C191
Working Life 25.0 min
Shelf Life 12.0 Month
@Temperature 4.00 - 30.0 °C
in original unopened cartridge
 
Descriptive Properties
ColorConcrete gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Portland Cement with Treated Silica Fume
Concrete, Highstrength
Concrete; Stone, 1-2-4 Mix
Portland Cement with Untreated Silica Fume
Concrete, gravel or crushed stone aggregate

PSIKA909 / 209816

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.