MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218W V15 PA66, 15% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Description: Polyamide 66, reinforced with 15% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.

Available in: North America

Product Applications: TECHNYL ® a 218W V15 is used in all sectors of industry, offering an excellent combination of thermal and mechanical properties. This grade is recommended for the production of mechanical components in permanent or intermittent contact with hot water: e.g. electro-magnetic valves. This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183/A
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed Arlon® 1163 PEEK, Glass Filled
Gharda Chemicals GATONE™ PEEK, 30% Glass Reinforced
Evonik VESTAKEEP® 4000GF30 PEEK
E-Polymers TEKAMID® TA210G15 , 15% Glass Fiber Reinforced PA66, DAM
EMS-Grivory Grivory® HTV-6H1 nat PA6T/6I-GF60

PRHOD677 / 137908

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.