PREBLACK PE 716-40 is a polyethylene based black masterbatch. It has been developed for the coloring of thicker PE-LD, PE-LD, PE-LLD and PE-HD films. It is also well suited for coloring of injection molded and extruded products made out of polyolefines. PREBLACK PE 716-40 gives also an antiblock effect and is therefore a good choice when producing films from recycled raw materials. Information provided by Premix Thermoplastics Inc. |