MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ChevronTexaco RPM® SAE 85W-140 Universal Gear Lubricant
Categories: Fluid; Lubricant

Material Notes: Features

Chevron RPM Universal Gear Lubricants are multipurpose lubricants.

They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life. The sulfur-phosphorus extreme pressure additives used in Chevron RPM Universal Gear Lubricants provide superior thermal and oxidation stability.

In addition, this lubricant is fortified with rust and corrosion inhibitors, a foam inhibitor, and a pour point depressant.

It also contains a friction modifier that allows its use as a top-off lubricant in gear cases with limited-slip or positrack differentials.

The sulfur-phosphorus extreme pressure additives in Chevron RPM Universal Gear Lubricants reduce the spalling and wear of gears by creating a microthin sacrificial film on the surface of the gear teeth which is actually softer than the gears themselves. Frictional heat and pressures between tooth surfaces cause the sulfur-phosphorus to react with the surface of the gear teeth at the point of contact, thus creating the sacrificial film.

The highly refined base stocks and various inhibitors in the additive package assure a well-balanced lubricant and long gear and bearing life.

Applications

Chevron RPM Universal Gear Lubricants are recommended for use in all spiral bevel and hypoid differentials, power dividers, and oil-lubricated steering axle wheel bearings.

Their multiviscosity characteristics allow their use in equipment operating over a broad ambient temperature range. This means good cold flow properties and gear protection.

Chevron RPM Universal Gear Lubricants:

  • meet the performance requirements of API Service Categories MT-1, GL-4 and GL-5
  • are qualified for SAE J 2360 (formerly known as MIL-PRF-2105E)
  • have Mack GO-J approval
  • meet the requirements (discontinued in 1998) of the U.S. Department of Agriculture (USDA) for use in federally inspected meat and poultry plants as H2 lubricants with no food contact.

Key Words: CPS Number: 225039; MSDS Number: 7234
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 25.9 °
Brookfield Viscosity 102000 cP
@Temperature -12.0 °C
Viscosity Measurement 95Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1719 SUS
Saybolt Viscosity at 210°F 124 SUS
Kinematic Viscosity at 40°C (104°F) 341 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 25 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Timken Test 65.0 lb
 
Thermal PropertiesOriginal ValueComments
Pour Point -15.0 °CASTM D97
Flash Point 229 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips 66 Inca® 1000 Oil, AGMA No. 8A Comp.
Phillips 66 680 Bearing Oil
Karina E TR 500D22/173 Honey PVC Compound
Honeylocust Wood
ChevronTexaco SAE 75W-90 Manual Transaxle Fluid GL-4

WCHEV220 / 74835

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.