MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DayGlo Gem-Tone GC-13P Ruby Red
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Gem-Tone® GC-13P Ruby Red is a rich, strong blue shade red colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of this colorant. No blooming or plateout problems will be seen with Gem-Tone® colorants. These materials can be incorporated into polyolefin resins at levels as low as 0.05% and can be increased to higher levels to achieve the desired effect.

Key Words: Pigment; Colorant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/cc
Bulk Density 32.0 lb/ft³
Oil Absorption 53 %
Particle Size 20 - 80 µm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 550 °F
Softening Point 90.0 - 100 °C
Glass Transition Temp, Tg 76.0 °C
Decomposition Temperature 318 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= 350 °F
 
Descriptive Properties
λmax519nmAbs. = 11300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Goodfellow Ruby, Al2O3
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
Superior Flux Ruby Fluid Stainless Steel General Purpose Soft-Soldering Flux
Mateck Sapphire (Al2O3)

PDAYGLO19 / 29560

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.