Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate components and give good selfleveling and air release. It has very good resistance to water, acids and bases, and most organic solvents. It was especially formulated to a 1A:1B mix ratio for use in automatic mixing equipment and dispensers with static mixers. EP1305LV Black will reach handle cure at room temperature within 2 – 4 hours, full cure in 24 hours. Cure time can be accelerated by the application of heat. Times and temperatures from 2 hours at 65°C to 1 hours at 100°C are typical for most applications. Cooler temperatures will also extend work time and increase cure times.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company. |