MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV X6145N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X6100 series are engineered materials designed for consumer, automotive, and industrial applications requiring superior Colorability and elastic performance. This product is a medium hardness, low density, multi-purpose thermoplastic vulcanizate that does not require pre-drying and can be processed by injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Flow; Good Processability; Medium Hardness; Low Density; Low Specific Gravity; Resilient

Uses: Automotive Applications; Consumer Applications; Industrial Applications; Rubber Replacement; Soft Touch Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccISO 1183
Viscosity 225 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 42
@Time 5.00 sec
Extruded; ISO 868
 46
@Time 5.00 sec
Injection Molded; ISO 868
Tensile Strength at Break 450 psiFlow; ISO 37
 537 psiAcross Flow; ISO 37
Tensile Stress at Strain 160 psi
@Strain 100 %
Across Flow; ISO 37
 232 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 400 %Flow; ISO 37
 610 %Across Flow; ISO 37
Tear Strength 90.0 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set 24 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 33 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 49 %
@Temperature 125 °C,
Time 252000 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 360 - 440 °F
Rear Barrel Temperature 280 - 320 °F
Middle Barrel Temperature 330 - 380 °F
Front Barrel Temperature 350 - 440 °F
Nozzle Temperature 360 - 440 °F
Mold Temperature 60.0 - 130 °F
Back Pressure 50.0 - 150 psi
Screw Speed 25 - 75 rpm
 
Descriptive Properties
AppearanceNatural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
E-Polymers EFLEX® V2045 SEBS/TPV
Chengdu Polyster 4502 High Performance Grade TPV
Barlog Plastics KEBAFLEX E 50.1 TPE-V, Shore A50
Barlog Plastics KEBAFLEX E 45.1 TPE-V, Shore A45
Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40

PTEKNQ1214 / 237705

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.