MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reynolds XTC-3D® High Performance 3D Print Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: XTC-3D™ is a protective coating for smoothing and finishing 3D printed parts. It does not melt plastic. Two liquids are mixed together and brushed onto any 3D print. Coating self-levels and wets out uniformly without leaving brush strokes. Working time is 10 minutes and cure time is about 4 hours (depending on mass and temperature). XTC-3D™ cures to a hard, impact resistant coating that can be sanded, primed and painted. Adding colors and metal effects is easy. Inexpensive to Use – 1 oz covers 100+ square inches (see coverage information below). 90% Time & Labor Savings: XTC-3D™ fills in 3D print striations and creates a smooth, high gloss finish. The need to post finish is almost eliminated. Coat any 3D Print Surface - XTC-3D™ can be applied to both SLA and SLS prints. It works with PLA, ABS, Laywoo, Powder Printed Parts and other rigid media. It also can be used to coat EPS, EPDM and urethane foam as well as wood, plaster, fabric, cardboard and paper. XTC-3D™ does not contain VOC’s, phthalates or phosphates.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D-1475
Viscosity 350 cPMixed; ASTM D-2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D-2240
 
Processing PropertiesOriginal ValueComments
Cure Time 1.50 hourThin Film Tacky Recoat Time
 2.00 hourThin Film, Tack Free Time
 3.50 hour
 20.0 minThin Film Working Time
Pot Life 10.0 minASTM D-2471
 
Descriptive Properties
ColorClear
Mix Ratio100A:42Bby weight
 2A:1Bby volume
Specific Volume25.1[in3/lb]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN208 / 296909

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.