MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Avient Nymax™ GF 1800 35 HS Natural Polyamide 612 (Nylon 612)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Property data for molded test bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 35 %Unspecified
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 160 MPaISO 527-2/5
Flexural Modulus 7200 MPaISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²ISO 180
 
Descriptive Properties
AdditiveHeat Stabilizer
AppearanceNatural Color
Filler / ReinforcementGlass Fiber Reinforcement
FormsPellets
Generic MaterialNylon 612
Generic NamePolyamide 612 (Nylon 612)
Regional AvailabilityNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nylene® 8100 Unfilled Nylon 6/12
Global EPP PA 612 Copolymer Cast Polyamide 612
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized
Ashley Polymers Ashlene® 981S Nylon 612
Arkema Rilsamid® DESNO PA612

PH0POL1437 / 146006

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.