MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
AISI 8642H Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, round
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Key Words: UNS H86420, ASTM A304, SAE J1268
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 285
@Diameter 102 mm
 306
@Diameter 76.2 mm
 331
@Diameter 50.8 mm
 363
@Diameter 25.4 mm
Hardness, Knoop 311
@Diameter 102 mm
Converted from Brinell
 333
@Diameter 76.2 mm
Converted from Brinell
 359
@Diameter 50.8 mm
Converted from Brinell
 392
@Diameter 25.4 mm
Converted from Brinell
Hardness, Rockwell B 99
@Diameter 50.8 mm
Converted from Brinell
 99
@Diameter 76.2 mm
Converted from Brinell
 99
@Diameter 102 mm
Converted from Brinell
 100
@Diameter 25.4 mm
Converted from Brinell
Hardness, Rockwell C 30
@Diameter 102 mm
Converted from Brinell
 33
@Diameter 76.2 mm
Converted from Brinell
 36
@Diameter 50.8 mm
Converted from Brinell
 40
@Diameter 25.4 mm
Converted from Brinell
Hardness, Vickers 301
@Diameter 102 mm
Converted from Brinell
 323
@Diameter 76.2 mm
Converted from Brinell
 350
@Diameter 50.8 mm
Converted from Brinell
 384
@Diameter 25.4 mm
Converted from Brinell
Tensile Strength, Ultimate 972 MPa
@Diameter 102 mm
 1040 MPa
@Diameter 76.2 mm
 1125 MPa
@Diameter 50.8 mm
 1240 MPa
@Diameter 25.4 mm
Tensile Strength, Yield 814 MPa
@Diameter 102 mm
 889 MPa
@Diameter 76.2 mm
 986 MPa
@Diameter 50.8 mm
 1110 MPa
@Diameter 25.4 mm
Elongation at Break 15 %
@Diameter 25.4 mm
in 50 mm
 16.8 %
@Diameter 50.8 mm
in 50 mm
 18.2 %
@Diameter 76.2 mm
in 50 mm
 19.2 %
@Diameter 102 mm
in 50 mm
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Calculated
Machinability 65 %annealed and cold drawn. Based on AISI 1212 steel = 100%.
Shear Modulus 80.0 GPaTypical for steel.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000234 ohm-cmTypical steel
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.475 J/g-°CTypical steel
Thermal Conductivity 46.6 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.39 - 0.46 %
Chromium, Cr 0.35 - 0.65 %
Iron, Fe 96.465 - 97.91 %As remainder
Manganese, Mn 0.70 - 1.05 %
Molybdenum, Mo 0.15 - 0.25 %
Nickel, Ni 0.35 - 0.75 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.30 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 8642 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, round
AISI 8642 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, round
AISI 8640 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 100 mm (4 in.) round
AISI 8640 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 75 mm round
AISI 8640 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 50 mm (2 in.) round

M864DA / 8494

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.