MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
202 Stainless Steel, Annealed Sheet, longitudinal orientation
Categories: Metal; Ferrous Metal; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: High-Nitrogen Austenitic Stainless Steel. Low-nickel equivalent of AISI Type 302.

Information provided by Chevron-Phillips Chemical Company, LLC and the references.

Key Words: UNS S20200
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.86 g/ccEstimated from similar materials
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 705 MPa
@Temperature 24.0 °C
 1080 MPa
@Temperature -73.0 °C
 1420 MPa
@Temperature -268 °C
 1590 MPa
@Temperature -196 °C
Tensile Strength, Yield 325 MPa
@Temperature 24.0 °C
 485 MPa
@Temperature -73.0 °C
 610 MPa
@Temperature -196 °C
 765 MPa
@Temperature -268 °C
Elongation at Break 25 %
@Temperature -268 °C
 41 %
@Temperature -73.0 °C
 52 %
@Temperature -196 °C
 57 %
@Temperature 24.0 °C
Modulus of Elasticity 207 GPaEstimated from similar materials
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.500 J/g-°CEstimated from similar materials
Thermal Conductivity 16.3 W/m-KEstimated from similar materials
Melting Point 1400 - 1450 °CEstimated from similar materials
Solidus 1400 °CEstimated from similar materials
Liquidus 1450 °CEstimated from similar materials
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 17 - 19 %
Iron, Fe 68 %As remainder
Manganese, Mn 7.5 - 10 %
Nickel, Ni 4.0 - 6.0 %
Nitrogen, N <= 0.25 %
Phosphorus, P <= 0.060 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
202 Stainless Steel, Annealed Plate, Sheet, Strip
202 Stainless Steel, Annealed Bar
304 Stainless Steel
AK Steel 304 Austenitic Stainless steel
202 Stainless Steel, 50% cold reduced sheet, longitudinal orientation

MQ202H / 171849

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.