MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Von Roll AR 600 T23 Epoxy - Aramid Fiber Laminate
Categories: Polymer; Thermoset; Epoxy

Material Notes: Highlights: Good slide and wear resistance together with high mechanical resistance, low coefficient of linear expansion, low density. Applications: slides

Synthetic fiber laminates are made without glass and are manufactured using high-pressure techniques. They are characterized by extremely high mechanical strength, a low friction coefficient and excellent abrasion resistance. Synthetic fiber laminates are used to make slides in high-performance rotary vacuum pumps and compressors, glide rods and friction discs – as well as operating rods in SF-6 circuit breakers, and wherever a high modulus of elasticity in tension is required.

Information provided by Von Roll.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
 
Descriptive Properties
ReinforcementAramid fabric
Sheet Sizes (mm)1150 x 1000, 2050 x 1000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVONR9920 / 249210

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.