MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® UA 2856 XP Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Aliphatic, acrylate-modified polyurethane dispersion. Binder for waterborne, air- and oven-drying basecoats in two-layer systems for automotive coatings, coatings for plastics, automotive refinishing coatings, industrial coatings and stone chip functional coatings.

Properties / Applications: When used in two-layer systems with TSA and two-component polyurethane clearcoats, metallic basecoats formulated with Bayhydrol® UA 2856 XP are characterized by even, cloud-free films with a very good flop effect, excellent gloss and good hiding power. The metallic basecoat can be oversprayed with TSA or two-component polyurethane clearcoats after pre-drying e.g. for 5 min at an oven temperature of 80 °C. Based on its high flexibility Bayhydrol® UA 2856 XP is also suitable as a binder for coatings that are highly resistant to stone chipping, such as stone chip primers.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccDIN EN ISO 2811
Volatiles 64 - 66 %1g/1h/125°C; DIN EN ISO 3251
pH 6.5 - 8.010% in demin. Water; DIN ISO 976
Viscosity <= 100 cPD= approx. 41.29 s-1; DIN EN ISO 3219/A.3
 
Descriptive Properties
Appearancedispers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0170 / 201953

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.