MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
KLJ Group KANATOL 3200 C Plasticizer
Categories: Fluid

Material Notes: Properties: K-3200C is a colorless, transparent oily liquid, slight sweet odour. It helps to get Insoluble Organic UV filters dispersed in high concentrations.

Application: As a solvent, diluents and fixative by the perfumers. An excellent active agent for Deodorants as it inhibits the enzymatic decomposition of the sweat components. A Phthalate free solvent for Cellulose/Cellulose compounds & paints. K-3200C itself is a permitted food additive (E1505) as a carrier for flavors. In the manufacture of insecticides and mosquito repellants. As alcohol denaturant. Excellently compatible with new resin systems used in the manufacture of low volatile hair sprays. In modern sun cream formulations. K-3200C is approved within the relevant pharmacopoeia. It is used for medical and pharmaceutical applications. Enteric coatings for controlled release tablets with K-3200C provide an optimized glass transition temperature which allows lower levels of addition.

Chemical Name: Tri Ethyl Citrate

Molecular Formula: C 12 H20 O7

Molecular Structure: (C2 H5COO) 3 .(C3 H4 OH)

CAS Number: 77-93-0

EINECS NO.: 201-070-7

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.134 - 1.14 g/cc
@Temperature 27.0 °C
ASTM D1045-08
Viscosity 32 - 38 cPKLJ TM-P-13-97
Molecular Weight 276.3 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 127 °C
@Pressure 0.00132 MPa
IS 5298-05
Flash Point 150 °CCOC
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.442 - 1.448
@Temperature 27.0 °C
ASTM D1045-08
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.030 %ASTM E203-08
Shelf Life 24.0 Month
 
Descriptive Properties
Acidity after heat treatment<0.6%180°C for 2 hrs, ISI-9591-03
Acidity as Acid<0.02%ASTM D1045-08
AppearanceWater White Clear Liquid
Color<40Hazen, ASTM D1045-08
Content>99%Ester Content, ASTM D1045-08
 >99%Plasticizing Ester by GLC, KLJ TM-P-12-98
 516-522 mg KOH/gmEster Value, ASTM D1045-08
Heat Stability45 Huat 150°C for 2 hrs, ISI-9591-03
Volatile Loss<0.2%110°C for 1 hrs, KLJ TM-P-11-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ245 / 284266

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.