MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos N12Z-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: N12Z-00 impact copolymer polypropylene is a medium melt flow rate, nucleated and antistatic product designed for injection molding applications. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.
    Applications:
  • Housewares, consumer goods including storage container and lids
  • Appliance housings
  • Rigid packing requiring exceptional toughness
  • Material handling products (crates and pails)
    Benefits:
  • High impact resistance
  • Very good stiffness
  • Excellent mold release
  • Good static dissipation

Information provided by Ineos Olefins & Polymers USA

Key Words: Medium melt flow rate, nucleated and antistatic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.903 g/ccASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 66ASTM D785
Tensile Strength at Break 2610 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 3260 psi2.0 in/min; ASTM D638
Elongation at Break 380 %2.0 in/min; ASTM D638
Elongation at Yield 6.6 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 154000 psiASTM D790A
Izod Impact, Notched 1.70 ft-lb/in
@Temperature -20.0 °C
ASTM D256
Izod Impact, Notched (ISO) 4.24 ft-lb/in²
@Temperature -20.0 °C
Area; ASTM D256
 NB
@Temperature 22.8 °C
Area; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 201 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °FUnannealed; ASTM D648
Vicat Softening Point 291 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 68 %60°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Dynatup Instrumented ImpactDuctile23°C, mode of failure
 Ductile-20°C, mode of failure
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem 5E16S Polypropylene Homopolymer
Ineos 3950 Polypropylene Impact Copolymer
Braskem 52T30V Homopolymer Polypropylene
BP Amoco Amoco® Polypropylene Homopolymer
Borealis RF926MO Polypropylene, Transparent Random Copolymer

PINEOS909 / 130368

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.