MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SnEco, Copper Alloy, UNS C69310, H00 Temper, Rod & Bar
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/8 Hard

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Hot Formed; Good Suitability – Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Poor Suitability – Capacity for Being Cold Worked

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.300 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 85
@Thickness 25.4 mm
Tensile Strength >= 69.6 ksi
@Thickness 25.4 mm
 87.0 ksi
@Thickness 25.4 mm
Typical
Tensile Strength, Yield >= 34.8 ksi
@Thickness 25.4 mm
0.2% Offset
 43.5 ksi
@Thickness 25.4 mm
0.2% Offset, Typical
Elongation at Break >= 10 %
@Thickness 25.4 mm
Tensile Modulus 15200 ksi
Modulus of Rigidity 5714 ksiCalculated
Poissons Ratio 0.33
Machinability 70 %
Forgeability 95 %
Impact Test 9.20 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000220 ohm-cm8% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µin/in-°F
@Temperature 20.0 - 100 °C
 10.3 µin/in-°F
@Temperature 20.0 - 200 °C
 10.4 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 21.7 BTU-in/hr-ft²-°F
Melting Point 1562 - 1652 °F
Solidus 1562 °F
Liquidus 1652 °F
Annealing Point 932 - 1112 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 74 - 79 %
Iron, Fe <= 0.10 %
Lead, Pb <= 0.090 %
Manganese, Mn <= 0.10 %
Nickel, Ni <= 0.20 %
Phosphorus, P 0.040 - 0.15 %
Silicon, Si 2.6 - 3.4 %
Tin, Sn 0.30 - 0.70 %
Zinc, Zn 16.4 - 23.1 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC69310x1 / 292378

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.