BL 20/1 GG EP is a composite bearing material that combines the crucial parameters for rotary blades. These include compressive stability at high temperatures, impact strength, low swelling and low coefficient of friction and expansion in conjunction with excellent wear characteristics. Information provided by Brandenburger Isoliertechnik GmbH&Co. |