MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ 124R PC (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility information and should not be used for medical applications which require biocompatibility. Alternative grade HP2.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 1.20 g/ccASTM D792
Density 1.19 g/ccASTM D792
Water Absorption 0.15 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.35 %ASTM D570
 0.58 %
@Temperature 100 °C
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 17.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 65.0 MPa50 mm/min; ISO 527
 68.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa50 mm/min; ASTM D638
 63.0 MPa50 mm/min; ISO 527
Elongation at Break 100 %50 mm/min; ISO 527
 125 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ISO 527
 7.0 %50 mm/min; ASTM D638
Tensile Modulus 2350 MPa1mm/min; ISO 527
 2370 MPa50 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 96.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2340 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 694 J/mASTM D256
Izod Impact, Unnotched 3204 J/mASTM D4812
Izod Impact, Notched (ISO) 12.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 35.0 kJ/m²ISO 179/2C
Tensile Impact Strength 546 kJ/m²ASTM D1822
Dart Drop, Total Energy 62.0 Jpeak; ASTM D3763
Falling Dart Impact 169 JASTM D3029
Taber Abrasion, mg/1000 Cycles 10CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
 >= 1.00e+17 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
 2.7
@Frequency 1e+6 Hz
IEC 60250
 2.96
@Frequency 1e+6 Hz
ASTM D150
 3.17
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 14.9 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 30 - 60 secUL 746A
High Amp Arc Ignition, HAI 60 - 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Specific Heat Capacity 1.25 J/g-°CASTM C 351
Thermal Conductivity 0.190 W/m-KASTM C177
 0.200 W/m-KISO 8302
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 133 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 137 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 129 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 140 °CRate B/50; ISO 306
 141 °CRate B/120; ISO 306
 154 °CRate B/50; ASTM D1525
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 HB
@Thickness 1.47 mm
UL 94
Oxygen Index 25 %ISO 4589
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
Haze 1.0 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 88 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 300 °CInjection Molding
Zone 1 260 - 280 °C
Zone 2 270 - 295 °C
Zone 3 280 - 305 °C
Melt Temperature 280 - 305 °C
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10396 / 243863

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.