MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Borealis WG320C Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: WG320C is a polypropylene for extrusion coating. Applications: microwave oven applications, pinholes free coating, extrusion coating of high volume production of boards and papers, coating of textile fibers, coating of various plastic films and cellophane, paper lamination films, and coating and lamination of aluminum foil.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccISO 1183
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Neck In 8.00 cmBTM 00115
Coating Weight >= 12.0 g/m²BTM 00117
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 147 °C
@Load 1.02 kg
A50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis WG341C Polypropylene
Ineos N00GX11 Polypropylene Impact Copolymer
Ineos H05H-01 Polypropylene Homopolymer
Ineos H03G-02 Polypropylene

PBOREA607 / 108866

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.