PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has an excellent balance of mechanical properties with good impact strength. PRE-ELEC 12-000 is easy to extrude or injection mold. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc. |