MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC XENOY™ X4830 PC+PBT (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: XENOY X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional stability. The X4830 could be positioned for body panels, safety equipment, housings, doorhandles, spring-loaded applications, medical device enclosures, outdoor sports equipment.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Density 1.27 g/ccISO 1183
Water Absorption 0.42 %23°C/sat; ISO 62
Moisture Absorption 0.140 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 7.0 g/10 min
@Load 5.00 kg,
Temperature 266 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 105 MPaISO 2039-1
Tensile Strength at Break 55.0 MPa50 mm/min; ISO 527
 60.0 MPa50 mm/min; ASTM D638
 60.0 MPa5 mm/min; ISO 527
 60.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa5 mm/min; ISO 527
 56.0 MPa5 mm/min; ASTM D638
 60.0 MPa50 mm/min; ASTM D638
 61.0 MPa50 mm/min; ISO 527
Elongation at Break 110 %50 mm/min; ISO 527
 120 %5 mm/min; ISO 527
 140 %50 mm/min; ASTM D638
 150 %5 mm/min; ASTM D638
Elongation at Yield 4.1 %50 mm/min; ASTM D638
 4.1 %5 mm/min; ISO 527
 4.2 %50 mm/min; ISO 527
 4.5 %5 mm/min; ASTM D638
Tensile Modulus 3200 MPa1mm/min; ISO 527
 3400 MPa5 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 96.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2900 MPa2 mm/min; ISO 178
 3100 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 600 J/mASTM D256
 120 J/m
@Temperature -30.0 °C
ASTM D256
 150 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Notched (ISO) 45.0 kJ/m²80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 40.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 70.0 JASTM D3763
 70.0 J
@Temperature -20.0 °C
ASTM D3763
Impact Test 110 JMultiaxial Impact; ISO 6603
Taber Abrasion, mg/1000 Cycles 30CS-17, 1 kg; SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 72.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 82.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 119 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 125 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 106 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 133 °CRate B/50; ASTM D1525
 133 °CRate B/50; ISO 306
 135 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 250 - 265 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 265 °C
Zone 3 250 - 270 °C
Melt Temperature 255 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10852 / 244319

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.