MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Phillips 66 595 NC Open Gear Lube
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Open Gear Lube 595 NC is a black, viscous, semi-fluid product that can be applied via central pumping systems that utilize injectors and nozzles for spray or drip application. Open Gear Lube 595 NC does not contain chlorinated solvents. Open Gear Lube 595 NC is designed for the lubrication of open gears, racks and pinions, swing gears, booms and sticks contained on mine and quarry shovels, drag lines and related equipment. Open Gear Lube 595 NC will perform over a wide temperature range above 15°F. The product will form a tenacious film that contains adhesive, extreme pressure properties, lubricity, rust and corrosion inhibitors and solid phase lubricating additives to provide maximum performance. Moreover, the lubricant resists water wash off and corrosion. Open Gear Lube 595 NC is removable and cleanable from decks, ladders and operating areas with wiping rags and conventional solvents or cleaning chemicals. The product is not the conventional heavy, tacky type that is extremely difficult and costly for maintenance removal.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccASTM D-1298
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 400 kgASTM D-2596
Four Ball Wear 0.500 mmASTM D-2296
Timken Test 45.0 lbASTM D-2509
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air 15.0 °F
Flash Point >= 300 °F
 
Descriptive Properties
AppearanceViscous, Semi-Fluid
ColorBlack
Cone Penetration325Undiluted, ASTM D217
Copper Corrosion1BASTM D130
Diluent Content8 wt. %
RustPassASTM D665 (24hrs at 60°C)
VentmeterMax 600 psigLincoln VE-1 (at 40°F)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON149 / 75186

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.