Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in Seconds Multi-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products form structural strength bonds to glass, metal and many filled plastic substrates in seconds.
Dymax 628 Structural Adhesive Moisture resistant; resilient and shock absorbing Key Substrates: Glass, filled plastics Typical Use: Electrical potting and tacking; keyless entry |