High flow and good impact performance. Natural and colored Polycarbonate based compound meant for furniture, electrical appliances, and technical lighting. These compounds are used mainly in the automotive and household industry to manufacture outer casings and protection guards, in the furniture sector to manufacture chairs, for the production of footwear, and for the production of sport articles such as helmets, ski boots, and roller blades. Information provided by SO.F.TER. Spa |