MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 253-15 GHIU Nylon 6, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Notes: 253-15 GHIU is a 15% glass fiber reinforced, impact modified nylon 6 that offers good mechanical performance coupled with good surface finish. It is heat & UV stabilized so that the good mechanical performance and surface appearance is maintained when exposed to high service temperature and weathering resistance. Color change after 2500 kj/m3 exposure (SAE J1960) <3 Delta E

Availability: Europe

Fillers/Reinforcement: Glass Fiber, 15% Filler by Weight

Additive: Heat Stabilizer; Impact Modifier; UV Stabilizer

Features: Good Surface Finish; Heat Stabilized; Impact Modified; Light Stabilized; Weather Resistant

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
Moisture Absorption at Equilibrium 2.2 %50% RH; ISO 62
Linear Mold Shrinkage 0.0080 - 0.015 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13800 psiISO 527-2
Elongation at Break 4.0 %ISO 527-2
Elongation at Yield 3.0 %ISO 527-2
Flexural Strength 18100 psiISO 178
Flexural Modulus 580000 psiISO 178
Izod Impact, Notched (ISO) 6.20 ft-lb/in²ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Dielectric Strength 280 V/mil
@Thickness 3.00 mm
IEC 60243-1
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µin/in-°F
Deflection Temperature at 0.46 MPa (66 psi) 383 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 365 °FUnannealed; ISO 72-2/A
Oxygen Index 22 %ISO 4589-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 464 - 518 °F
Middle Barrel Temperature 464 - 518 °F
Front Barrel Temperature 464 - 518 °F
Melt Temperature 464 - 518 °F
Mold Temperature 140 - 176 °F
Drying Temperature 176 °F
Dry Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0514 / 237005

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.