MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Powersil® GEL C 670 A/B Silicone Gel
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® GEL C 670 A/B is a two-component, addition-curing silicone rubber that cures at room temperature to a soft silicone gel.

Special features:

  • two-part, 1 : 1 mixing ratio
  • compressibility
  • low density
  • low viscosity
  • no harmful effects known
  • easy metering
  • easy to mix
Application:
  • filling of cable terminations
  • filling of bushings
  • filling of electrical equipment

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.700 g/ccISO 1183-1 A
Viscosity 3000 cPComponent A; ISO 3219
 3000 cPComponent B; ISO 3219
 4000 cPMixed; ISO 3219
 
Mechanical PropertiesOriginal ValueComments
Penetration 220
@Load 0.150 kg
1/10 mm, hollow cone; ISO 2137
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.0
@Frequency 50 Hz
IEC 60250
Dielectric Strength 18.0 kV/mmIEC 60243
Dissipation Factor 0.00040
@Frequency 50 Hz
IEC 60250
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Treatment Temp. 150 °C
1cm
 8.00 hour
@Treatment Temp. 23.0 °C
1 cm
 30.0 min
@Treatment Temp. 150 °C
circulating air oven
Pot Life 140 min
 
Descriptive Properties
ColorwhiteComponent A
 whiteComponent B
 whitecured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9392 / 204921

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.