Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |