MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Brewer Science BrewerBOND® 220 Temporary Wafer Bonding Material
Categories: Other Engineering Material

Material Notes: BrewerBOND® 220 temporary wafer bonding material is an organic coating that enables back-end-of-line (BEOL) processing of ultrathin wafers using standard semiconductor equipment. This product improves throughput, simplifies cleaning, and shortens processing time.

For coatings thicker than 20 µm, BrewerBOND® 220 material is a good option as an alternative solution to typical wax adhesives. It offers significant advantages because it can be applied with a one-coat process. The material provides up to a 160-µm film with a single coat and customized spin process. BrewerBOND® 220 material enables backside temperature processing up to 250°C with minimal device wafer bowing. BrewerBOND® 220 material does not introduce additional stress in the bonded stack. This versatile material can be used for the thermal slide or mechanical debonding methods.

Benefits:

  • Enables backside temperature processing at 200°C – 240°C
  • Enables slide debonding with low force
  • Enables minimal device wafer bowing during processes
  • Up to 160-µm film possible with a single coat and customized spin process BrewerBOND® 220 Bonding Material Coating Parameters (8” substrate) Static dispense in center of wafer.

Information provided by Brewer Science.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 100000 cP
@Temperature 200 °C
Complex Melt Viscosity
 500000 cP
@Temperature 150 °C
Complex Melt Viscosity
 5.00e+6 cP
@Temperature 100 °C
Complex Melt Viscosity
 2.00e+10 cP
@Temperature 50.0 °C
Complex Melt Viscosity
Brookfield Viscosity 1480 cP
@Temperature 37.8 °C
 2828 cP
@Temperature 25.0 °C
Thickness 58.0 micronsSpin Speed 600 rpm
 110 micronsSpin Speed 300 rpm
 
Thermal PropertiesOriginal ValueComments
Transformation Temperature, Tg 50.1 °CDSC
Decomposition Temperature 254 °C2% wt loss in TGA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Gallium Arsenide Semiconductor Wafer, p-type, Zinc Doped, LEC Grown
Ditungsten Nitride, W2N
Aluminum Antimonide, AlSb
Mateck GaAs
Mateck Gallium Arsenide (GaAs)

PBREW990 / 193506

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.