MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Ceramics MICROSIL Microporous Insulation
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: MICROSIL Microporous Insulation is an insulation material. Having thermal conductivity an order of magnitude lower than ceramic fiber materials Microsil Microporous Insulation can be an integral part of thousands of thermal management applications with temperatures as high as 950C (1742F). MICROSIL is a combination of ultra-fine silica powders, specially processed refractory oxides and glass reinforcing fibers. Compacted under tons of force to form a light weight yet rigid structure MICROSIL offers maximum insulation in a minimum amount of space, saving weight and energy. Unique to MICROSIL's microporous structure is its low density which minimizes conductive heat transfer and its billions of nano-pockets which block convection and reflect heat energy – like mirrors – back to its source. MICROSIL is nearly immune to thermal shock. It is completely non-combustible in accordance with standard DIN 4102 Class A1 and can be stored indefinitely in dry conditions. MICROSIL's microporous structure is adversely effected by water, oil, alcohol and other liquids.

Information provided by Zircar.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.230 g/cc
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 1.10 MPaCold Crushing Strength
Compression Set 2.9 %Compression at 14 psi
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.190 BTU/lb-°F
@Temperature 20.0 - 800 °C
Thermal Conductivity 0.0190 W/m-K
@Temperature 20.0 °C
 0.0230 W/m-K
@Temperature 200 °C
 0.0280 W/m-K
@Temperature 400 °C
 0.0300 W/m-K
@Temperature 600 °C
 0.0380 W/m-K
@Temperature 800 °C
Maximum Service Temperature, Air 950 °C
Shrinkage 1.0 %
@Temperature 800 °C,
Time 86400 sec
 4.8 %
@Temperature 1000 °C,
Time 86400 sec
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.95
 
Component Elements PropertiesOriginal ValueComments
Other 5.0 %Oxides
SiC 15 %
SiO2 80 %
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elisto THERMOSTAR® LD 1000 Frame Press Insulation Material
Unifrax Excelfrax® 1800 Board Microporous Insulation
MarkeTech Silica Aerogel
Momentive Performance Materials "PG" Pyrolytic Graphite
Morgan Advanced Ceramics Alphawool® VF Board Thermal Ceramic

CZIR024 / 2832

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.