MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 5010 Polyurethane Multi-Purpose Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: 3M™ Polyurethane Multi-Purpose Adhesive 5010 is a one component, fast curing adhesive which forms a rigid permanent bond. 3M 5010 bonds to a wide variety of materials including wood, foam panels, fiberglass, and wood.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Volatile Organic Compounds (VOC) Content 2.1 g/l
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1.90 MPaASTM D412
100% Modulus 0.0117 GPa
@Strain 100 %
ASTM D412
Shear Strength 51.0 psiOverlap, Polypropylene
 90.0 psiOverlap, LD Polyethylene
 262 psiOverlap, Nylon
 333 psiOverlap, Glass
 357 psiOverlap, Polycarbonate
 492 psiOverlap, Acrylic
 528 psiOverlap, ABS
 686 psiOverlap, Fir
 790 psiOverlap, PVC
 905 psiOverlap, Aluminum
 1011 psiOverlap, Cold Rolled Steel
 1042 psiOverlap, Stainless Steel
 1668 psiOverlap, FRP Green
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -30.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 minPressing Time
 1440 minFinal Setting Time
Working Life 3.00 - 5.00 minOpen Time
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP-100 Epoxy Adhesive
3M Scotchkote™ HTX 517 Epoxy HT Lining
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Overview of materials for High Density Polyethylene (HDPE), Extruded
Permabond 731 Cyanoacrylate, toughened

PMM33163 / 167910

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.