MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lehvoss LUVOCOM® 1106-8465 Polyether imide with carbon fiber, thermally conductive modified
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), Carbon Fiber Filled

Material Notes: Properties/attributes include: Strong, stiff parts. High continuous-use and heat-distortion temperatures. Non flammable. Electrically conductive, suitable for continuous discharging of statically-generated electricity.

Typical uses include: Parts for electric and electronic industry, antistatic body parts

Processing: During processing the moisture level should not exceed 0.03%, otherwise porosity and surface defects (e.g. smearing) may occur. Predrying is recommended even when sealed original containers are being used. To avoid internal stresses, a low shear load should be used for processing. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccISO 1183
Moisture Absorption <= 0.200 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmDIN 16901
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 125 MPaISO 527-2
Elongation at Break 0.80 %ISO 527-2
Modulus of Elasticity 21.0 GPaISO 527-2
Flexural Strength 180 MPaISO 178
Flexural Modulus 18.0 GPaISO 178
Flexural Strain at Break 0.90 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 14.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eU
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1e+05IEC 60167
Surface Resistance <= 1e+05IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°CDIN 53752
Thermal Conductivity 6.00 W/m-K|| 60x60x3 mm; HOT-DISK
Maximum Service Temperature, Air 170 °CContinuous; UL 746B
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 350 - 400 °C
Zone 1 330 - 350 °C
Zone 2 340 - 390 °C
Zone 3 350 - 400 °C
Melt Temperature 380 °C
Mold Temperature 150 - 180 °C
Drying Temperature 120 °C
@Time >=28800 sec
Dehumidifying dryer
 150 °C
@Time >=14400 sec
Dehumidifying dryer
Moisture Content <= 0.030 %
 
Descriptive Properties
Colornatural color (black)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1301-7896 PPS, linear with carbon fiber, thermally conductive modified
Carlisle 201LL Carbon-Carbon Composite
Solvay Thornel® P-650/42 Carbon Fiber/Epoxy Advanced Composite System
Celanese CoolPoly® D5108 Thermally Conductive Polyphenylene Sulfide
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)

PLUU8857 / 193816

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.