MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer EXL1613T Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN EXL1613T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature ductility in combination with medium flow characteristics and excellent processability with opportunities for shorter IM cycle times compared to standard PC. LEXAN EXL1613T resin is a general purpose product available in transparent and opaque colors and is an excellent candidate for a broad range of applications.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Density 1.18 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0400 %23°C / 50% RH; ISO 62
Viscosity 7.5 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 8.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 47.0 MPa50 mm/min; ISO 527
 49.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 57.0 MPa50 mm/min; ASTM D638
 57.0 MPa50 mm/min; ISO 527
Elongation at Break 58 %50 mm/min; ASTM D638
 67 %50 mm/min; ISO 527
Elongation at Yield 5.7 %50 mm/min; ISO 527
 5.9 %50 mm/min; ASTM D638
Tensile Modulus 2100 MPa50 mm/min; ASTM D638
 2100 MPa1 mm/min; ISO 527
Flexural Strength 85.0 MPayield, 2 mm/min; ISO 178
 87.0 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 90.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2012 MPa1.3 mm/min, 50 mm span; ASTM D790
 2100 MPa2 mm/min; ISO 178
Izod Impact Notched 900 JASTM D256
 690 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 62.0 kJ/m²80*10*3; ISO 180/1A
 20.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) 130 kJ/m²80*10*3; ISO 180/1U
 130 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched 95.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eU
 95.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 70.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 20.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 75.0 JASTM D3763
 73.0 J
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 71.5 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 77.1 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 76.1 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 82.6 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 122 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 122 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 142 °CRate B/50; ISO 306
 143 °CRate B/120; ISO 306
 150 °CRate A/50; ASTM D1525
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.400 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Haze 1.3 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 87 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 300 - 320 °C
Zone 2 295 - 315 °C
Zone 3 305 - 330 °C
Melt Temperature 300 - 330 °CInjection Molding
Mold Temperature 80.0 - 115 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80184 / 288131

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.