MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Rykotac® Grease EP
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Features

Chevron Rykotac Grease EP is manufactured using highly refined, select high viscosity index base oils, and a polyurea thickener. It is red in color and tacky in texture.

Chevron Rykotac Grease EP contains polyurea thickener, highly refined paraffinic base oil, extreme pressure agents, and a special combination of synthetic tackiness agents. These agents allow maximum tackiness with a wide temperature range for high and low temperature performance.

Applications

Chevron Rykotac Grease EP is an excellent choice for heavy duty construction equipment, fifth wheel, chain drives, and other applications in which a grease that clings to metal and resists spin-off is needed. These properties are given by a formulation balanced to provide good cold weather and high temperature performance.

Chevron Rykotac Grease EP can be used in both plain and antifriction bearings.

Applications include:

  • Cement plants
  • Construction
  • Farming
  • Marine
  • Mining
  • Oil fields
  • Paper mills
  • General industry
  • Conveyor systems

Key Words: CPS Number: 231066; MSDS Number: 7813
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 171Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 741 SUS
Saybolt Viscosity at 210°F 106 SUS
Kinematic Viscosity at 40°C (104°F) 145 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 21 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Penetration 260Worked
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -34.0 °C
Dropping Point 260 °C
 
Descriptive Properties
ColorRed
TextureTacky
ThickenerPolyurea
Water Resistance, 79°C, % loss2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV266 / 74881

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.