MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Specialty Suspension CG E 24 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® CG E24 is a homopolymer specialty suspension resin intended for use in controlling gloss and transparency of injection molded, extruded or plastisol parts. This resin provides low surface gloss and texturing effects for flexible vinyl products, allowing the production of broad range of surface effects without the need for secondary operation process which helps to reduce manufacturing cost. Reduced gloss effects are created throughout the part wall, providing for the continued desired surface aesthetics. The ability to increase surface roughness provides a reduced surface blocking and allows the ease of handling in stacked or bundled parts.

Note: The value set forth represent 'typical' values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, netweight 50lbs, 2,500lbs per pallet. Information shown on the package includes commercial identification number, lot, and weight. STP 488 (formulation): 100phr Geon® CG E24, 55phr TOTM, and 18phr Filler

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Volatiles 0.10 %Geon® STP 793; Internal Method
Apparent Bulk Density 0.380 g/ccGeon® STP 1169; Internal Method
Porosity 0.53 %cm³/g; Geon® STP 1094; Internal Method
Particle Size <= 105 µm40%; Geon® DFT 1466; Internal Method
 125 µmAverage Particle Size Geon® DFT 1466; Internal Method
 >= 250 µm3%; Geon® DFT 1466; Internal Method
 
Descriptive Properties
Contamination0Internal Method; Magnetic Particles, Geon® STP 1217 Unit: #/100in2
 1Internal Method; Dark Particles, Geon® STP 1217 Unit: #/100in2
 9Internal Method; Light Colored Particles, Geon® STP 1217 Unit: #/100in2
FeaturesLow Gloss
 Non-Smooth Surface Finish
Flow Time32 secInternal Method; Conditioned Funnel Flow Time, Geon® STP 1169
FormsPowderWhite Powder
Generic MaterialPVC Homopolymer
Generic NamePolyvinyl Chloride Homopolymer (PVC Homopolymer)
Polymerization ProcessSuspension
Powder Mix Time3.3 minInternal Method; Geon® STP 488 (with provide formula)
Processing MethodDip Coating
 Extrusion
 Injection Molding
 Rotational Molding
 Slush Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Residual Vinyl Chloride Monomer< 1 ppmInternal Method; Geon® STP 1005
UsesInsulation
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH0POL1423 / 145992

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.