MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRIN™ WF006JiQ Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP ELCRIN WF006JiQ compound is based on Polybutylene terephthalate (PBT) resin utilizing ELCRIN iQ upcycling technology containing minimum 37% Post-Consumer Recycling (PCR) weight content and 30% glass fiber. Added features of this grade include: Low Extractables, Healthcare, Excellent Strength, Stiffness and Dimensional Stability.

Features: Post-Consumer Recycled (PCR) content,Low Extractable,Healthcare,High Stiffness,High Strength,Good dimensional stability,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/ccASTM D792
Density 1.54 g/ccISO 1183
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
 0.100 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.090 %ISO 62-1
Viscosity 38 cP
@Load 5.00 kg,
Temperature 250 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 52 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 114 MPa5 mm/min; ASTM D638
 139 MPa5 mm/min; ISO 527
Tensile Strength, Yield 114 MPa5 mm/min; ASTM D638
 139 MPa5 mm/min; ISO 527
Elongation at Break 1.6 %5 mm/min; ISO 527
 2.2 %5 mm/min; ASTM D638
Elongation at Yield 1.6 %5 mm/min; ISO 527
 2.2 %5 mm/min; ASTM D638
Tensile Modulus 10700 MPa1 mm/min; ISO 527
 11800 MPa5 mm/min; ASTM D638
Flexural Strength 189 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 210 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 210 MPayield, 2 mm/min; ISO 178
Flexural Modulus 9100 MPa1.3 mm/min, 50 mm span; ASTM D790
 9100 MPa2 mm/min; ISO 178
Izod Impact Notched 82.0 JASTM D256
 83.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 770 J/mASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 14.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 7.00 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Dielectric Strength 23.0 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 89.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 89.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 200 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 217 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 207 °C
@Thickness 6.40 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 265 °C
Zone 2 245 - 260 °C
Zone 3 250 - 265 °C
Melt Temperature 250 - 265 °CInjection Molding
Mold Temperature 65.0 - 90.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00250 - 0.00380 cm
Screw Speed 50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80617 / 288564

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.