MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Konson TMTM-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% tetramethylthiuram mono-sulphide, 20% EPDM/EVA binder and dispersing agents

Use Characteristics: A super accelerator Konson® TMTM-80 causes very rapid and scorch-safe vulcanization of natural and synthetic rubbers. Konson® TMTM-80 receives additional activation from basis accelerators, e.g. aldehyde amine and guanidine. Together with sulphenamide and mercapto accelerators in which Konson® TMTM-80 is used as secondary accelerator are of great technical importance. Low sulphur vulcanization provides vulcanizates with good ageing resistance.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective TMTM is assured.

Dosage levels: NR: primary: 0.15 - 0.3 phr + 2 - 3 sulfur secondary: 0.1 - 2.5 phr + 2.5 phr sulfur and 1 phr mercapto accelerator; SBR:primary: 0.25 - 1.5 phr + 2 - 3.5 phr sulfur secondary: 0.1 - 0.75 phr + 2 - 3.5 phr sulfur and 2 phr mercapto accelerator; IIR: primary: 1 - 2 phr + 1 - 2 phr sulfur; NBR: 0.1 - 3 phr + 0.5 - 2 phr sulfur and 1 - 2 phr mercapto accelerator; CR: 0.5 - 1 phr + 0.5 - 1 phr sulphur and 1 - 3 phr guanidine accelerator.

Applications: Cable insulations, light color and white vulcanizates, transparent pure rubber articles.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/cc
Ash <= 0.50 %
Evaporation Loss <= 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 100 °C
 
Descriptive Properties
AppearanceLight-yellow granules
Content= 98%TMTM
Sieve residue= 0.5 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS019 / 256064

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.