MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake 2082 Medium-low molecular weight, film and medical grade, PVC suspension resin
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded; PVC, Flexible Grade

Material Notes: Westlake 2082 is a medium-low molecular weight, film and medical grade, vinyl suspension resin. This resin has good clarity, color, plasticizer sorption and thermal stability. Kosher approved. Applications: Suited for flexible profile extrusion, extruded and calendered sheet, extruded foam profiles and other high flow, flexible profile applications.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.530 g/ccASTM D1895
Volatiles <= 0.35 %
Particle Mesh Size 40 Mesh> 99.9% Through; ASTM D1921
 200 Mesh< 7% Through; ASTM D1921
Viscosity Measurement 0.82Inherent; ASTM D5225
 
Descriptive Properties
AppearanceFree Flowing White Powder
Cell ClassificationGP3-16470ASTM D1755
K-Value62ISO1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWESF8754 / 287864

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.