MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sika Sikaflex® -2c Slope Grade Polyurethane elastomeric sealant
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Sikaflex-2c Slope Grade is a 2-component, premium-grade, polyurethane-based, elastomeric sealant comprised of various mixes of Sikaflex-2c SL and NS EZ Mix. Meets ASTM C-920, Type M, Grade SSL, Class 25, use T, NT, M, G, A, O.

Where to Use:

  • Intended for use in all properly designed working joints with a minimum depth of ¼ inch.
  • Ideal for sloped applications ranging from 10° to 50° slope.
  • Placeable at temperatures as low as 40°F.
  • Adheres to most substrates commonly found in construction.
  • Submerged environments, such as canal and reservoir joints.
Advantages:
  • Adjustable mixes for slope and workability preference
  • Chemical cure allows the sealant to be placed in non-moving joints exceeding ½ in. in depth.
  • High elasticity with a tough, durable, flexible consistency.
  • Exceptional cut and tear resistance.
  • Exceptional adhesion to most substrates without priming.
  • Available in 35 architectural colors.
  • Color uniformity assured via Color-pak system.
  • Easy to mix.
  • Paintable with water-, oil-, and rubber-base paints.
  • Jet fuel resistant.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20 - 45ASTM D2240
Tensile Strength at Break 95.0 - 175 psiASTM D412
Tensile Stress at Strain 70.0 - 100 psi
@Strain 100 %
Elongation at Break 300 - 650 %ASTM D412
Tear Strength 45.0 - 100 pliASTM D624
Peel Strength 15.0 - 30.0 pliConcrete, 0% Adhesion loss; Fed Spec. TT-S-00227E
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 170 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time >= 72.0 hourFinal cure
Tack-Free Time <= 6.00 hour10
Shelf Life 12.0 Month
@Temperature 4.00 - 35.0 °C
in original unopened cartridge
 
Descriptive Properties
ColorA wide range of architectural colors are available.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIKA924 / 209831

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.