MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
DSM Stapron® E EM 605 Polycarbonate/PET Blend (European Grade)  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Information provided by DSM.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
Water Absorption 0.35 %Sim. to ISO 62
Melt Flow 8.47 g/10 min
@Load 1.20 kg,
Temperature 280 °C
Calculated from Volume Flow Rate of 7 cm3/10min.; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPaISO 527-1/-2
Elongation at Break >= 50 %ISO 527-1/-2
Elongation at Yield 6.0 %ISO 527-1/-2
Tensile Modulus 2.20 GPaISO 527-1/-2
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 2.20 GPaISO 178
Izod Impact, Notched (ISO) 40.0 kJ/m²
@Temperature -40.0 °C
ISO 180/4A
 60.0 kJ/m²
@Temperature -20.0 °C
ISO 180/4A
 70.0 kJ/m²
@Temperature 23.0 °C
ISO 180/4A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 5.50 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 120 °CISO 75-1/-2
Vicat Softening Point 125 °C50°C/h 50N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 
Descriptive Properties
Heat Stabilized or Stable to HeatYes
High Impact or Impact ModifiedYes
Injection MoldingYes
Without FillersYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Covestro Bayblend® ET3036 FR PC/ABS Blend
LG Chemical LUPOY HR5007AE PC/ABS, High Impact
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Teijin Multilon T-3011 Standard PC/ABS Polymer Alloy

PDSMEU540 / 31391

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.