MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Tenite™ Propionate 360E4861312 Clear, Trsp Cellulosic Plastics
Categories: Polymer

Material Notes: Product Description: Tenite™ cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite™ cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite™ cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite™ Cellulosic Acetate Propionate 360-12has a plasticizer level of 12%. It is resistant to high temperatures.

Application/Uses:

  • Cosmetics/personal care packaging
  • Frames
  • Medical
  • Ophthalmics
  • Pen/stationary supplies
  • Toothbrushes
Key Attributes:
  • Ability to be solvent polished, cut, cemented, drilled, and decorated
  • Colorable—color concentrates available
  • Excellent clarity
  • Good chemical resistance
  • High surface gloss
  • Outstanding processability—easy to mold, extrude, or fabricate
  • Superior primary and secondary fabrication
  • Tough and durable
  • Warm feel

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 1.5 %24; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 33.1 MPaASTM D638
Tensile Strength, Yield 31.7 MPaASTM D638
Elongation at Break 45 %ASTM D638
Flexural Strength 41.4 MPaASTM D790
Flexural Modulus 1448 MPaASTM D790
Izod Impact, Notched 107 J/m
@Temperature -40.0 °C
ASTM D256
 416 J/m
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 - 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.3 - 3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 - 18.7 kV/mmASTM D149
Dissipation Factor 0.010 - 0.15
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 - 17.0 µm/m-°CASTM D696
Specific Heat Capacity 1.26 - 1.67 J/g-°C
Thermal Conductivity 0.170 - 0.330 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CASTM D648
Vicat Softening Point 96.0 °C
@Load 70.0 kg
ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46 - 1.49ASTM D542
Haze <= 8.5 %ASTM D1003
Transmission, Visible >= 90 %ASTM E308

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5607 / 222801

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.