MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Foam XP110
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The foam also possesses excellent dielectric properties. ULTEM foam is targeted at applications where structural fire performance, radar transparency, or extreme hot or cold environments are required. ULTEM foam is thermoformable and compatible with phenolic pre-pregs. Information on processing or secondary operations is available upon request.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.110 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2.10 MPain plane; ASTM D638
Tensile Modulus 40.0 MPain plane; ASTM D638
Compressive Strength 1.70 MPaperpendicular to plane; ASTM D1621
Compressive Modulus 103 MPaperpendicular to plane; ASTM D1621
Shear Modulus 0.0240 GPaASTM C273
Shear Strength 1.40 MPaASTM C273
Charpy Impact Unnotched 0.900 kJ/m²ISO R179
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0400 W/m-KASTM C518
Smoke Density <= 10Ds; FAR 25.853
 
Descriptive Properties
Insulation Radiant PanelPASSESFAR 25.856
OSU peak heat release rate (5 minute test)<55 kW/m²FAR 25.853
OSU total heat release (2 minute test)<55 kW-min/m²FAR 25.853
Smoke ToxicityPASSESOEM ABD
 PASSESOEM BSS
Vertical Burn at 60 SecondsPASSESFAR 25.853

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82772 / 290719

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.