MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® B 70 GFE 15 H PA6-GF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important properties:
  • High impact resistance
  • High stiffness
  • Good flowability
  • Good processability
Application examples are functional parts in automotive, structural components for furniture applications and housings for power tool.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDry; ISO 1183
Water Absorption 7.0 %Sim. to ISO 62
Moisture Absorption 2.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaConditioned; ISO 527-1/-2
 120 MPaDry; ISO 527-1/-2
Elongation at Break 3.5 %Dry; ISO 527-1/-2
 10 %Conditioned; ISO 527-1/-2
Tensile Modulus 3000 MPaConditioned; ISO 527-1/-2
 6000 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 70.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mmConditioned; IEC 60243-1
 35.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 500 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-1/-2
Melting Point 222 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °CLong Term; ISO 2578
 160 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 190 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 55.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveInterior
FormGranules
Industry & Consumer goodsHousewares
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Special CharacteristicsHigh impact or impact modified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® B 70 GFE 30 H PA6-GF30
LG Chemical LUMID HI2152A(W) PA6+GF15%, High Impact
Envalior Akulon® K224-HG3 PA6-GF15, Dry, 15% Glass Filled, Heat Stabilized
Envalior Akulon® K224-G3 PA6-GF15, Dry, 15% Glass Filled
EMS-Grivory Grilon® BGZ-15 PA6-GF15

PGRH160 / 156869

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.