Calprene 405 is a 67/33 Butadiene/Styrene thermoplastic copolymer, polymerized in solution. It has a radial structure. This product is presented in porous crumb form, which gives good oil absorption. Applications: Footwear Sportswear Mechanical rubber goods Bitumen modification Information provided by Dynasol. |