MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Sequel® E4000 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: Sequel E4000 thermoplastic polyolefin (TPO) is designed for extrusion applications that require high mechanical stiffness, thermal stability, good low-temperature properties, and good dimensional stability over a broad temperature range. This material can be supplied with or without UV stabilizers.

Availability: North America

Features: Good Dimensional Stability; Good Thermal Stability; High Resistance

Uses: Automotive Exterior Parts; Industrial Applications; Profiles

Processing Method: Extrusion; Thermoforming

Information provided by LyondellBasell Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183
Melt Flow 1.4 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3050 psi
@Thickness 3.99 mm
150x10x4 mm; ISO 527-2/50
Flexural Modulus 406000 psi
@Thickness 3.99 mm
80x10x4 mm; ISO 178
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 µin/in-°F
@Temperature -30.0 - 80.0 °C
ASTM E228
CTE, linear, Transverse to Flow 28.0 µin/in-°F
@Temperature -30.0 - 80.0 °C
ASTM E228

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLYON798 / 311491

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.