MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Controltac™ 180 Graphic Film
Categories: Polymer; Film

Material Notes: 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without rivets, simple curves, compound curves and corrugations; Film series 180C with Comply adhesive also have air release channels for fast and easy, bubble-free graphic installations; Film 180Cv2 (white only) features non-visible air release channels

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milwithout adhesive
 3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17.2 MPa
Peel Strength 3.00 - 4.00 pliAdhesion to Acrylic enamel
 3.00 - 5.00 pliAdhesion to Fruehauf pre-painted panels
 4.00 - 5.00 pliAdhesion to ABS
 4.00 - 5.00 pliAdhesion to Chrome
 5.00 - 6.00 pliAdhesion to Aluminum, etched
 7.00 - 8.00 pliAdhesion to Aluminum, anodized
 
Processing PropertiesOriginal ValueComments
Processing Temperature 4.00 - 38.0 °CApplication Temp; Flat surfaces without rivets
 16.0 - 32.0 °CApplication Temp; Compound curves
 10.0 - 38.0 °CApplication Temp; Curved or corrugated surfaces with rivets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thermal Ceramics Sonite 3000
Oxygen-free Electronic Copper (OFE), UNS C10100, O61 Temper Bar
Oxygen-free Electronic Copper (OFE), UNS C10100, H04 Temper, wire
Oxygen-free Electronic Copper (OFE), UNS C10100, H00 Temper, flat products
ELM® TempFlex™ 0 to 100 Biodegradable Rail Curve Lubricant

PMM34807 / 169554

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.