MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 76® Lubricants SAE Grade 40 Custom Motor Oil  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: 76® Custom Motor Oil is a high-quality automotive engine oil designed primarily for use in older (pre-1989) passenger cars and light trucks in light-duty service. It also is recommended for use in older (pre-1995) diesel equipment where an API CD quality oil is specified. It should not be used in engines where an oil meeting new car warranty requirements is required. Custom Motor Oil is formulated to provide good wear protection, to minimize the formation of sludge and varnish, to protect against rust and bearing corrosion, and to resist foaming.

Applications:

  • Automotive gasoline engines built prior to 1989 and operating under light-duty conditions
  • Older diesel equipment where API CD quality oil is specified
Custom Motor Oil meets or exceeds the requirements of:
  • API Service SF, CD
Features/Benefit:
  • Excellent oxidation resistance
  • Protects against sludge and varnish formation
  • Protects against wear
  • Protects against rust and bearing corrosion
  • Good foam resistance

Information provided by Phillips 66 Lubricants. The 76® Lubricants brand name was consolidated into other Phillips 66 brands in 2016; many products remain available under a new name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.875 g/cc
Density 7.29 lb/gal
Viscosity 3.9 cP
@Temperature 150 °C
High-Temp/High-Shear
Viscosity Measurement 101Index
Kinematic Viscosity at 40°C (104°F) 134 cSt
Kinematic Viscosity at 100°C (212°F) 14 cSt
Ash 0.79 %Sulfated; ASTM D874
ASTM Color 3.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Base Number 5.8ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -30.0 °C
Flash Point 246 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.089 %
Zinc, Zn 0.098 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON6388 / 210081

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.