MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Melinex® 6428 Polyester Film, 200 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 6428 is a high clarity polyester film. It is pretreated on both film surfaces to promote adhesion to EVA. Melinex® 6428 is a developmental film designed for the photovoltaics industry.

Also available as 650 Gauge

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.395 g/ccASTMD1505
Water Vapor Transmission 0.900 g/100 in²/day
@Temperature 38.0 °C
90% RH; ASTM F1249
Thickness 2.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 14000 psiASTM D882A
Film Tensile Strength at Yield, TD 14000 psiASTM D882A
Film Elongation at Break, MD 160 %ASTM D882A
Film Elongation at Break, TD 160 %ASTM D882A
Coefficient of Friction, Dynamic 0.40A-B; ASTM D1894
Film Tensile Strength at Break, MD 28000 psiASTM D882A
Film Tensile Strength at Break, TD 36000 psiASTM D882A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 5000 V/mil1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 10000 V1/4" electrode 500 V/sec 25°C in air; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 0.60 %
@Temperature 150 °C,
Time 1800 sec
Shrinkage, TD 0.60 %
@Temperature 150 °C,
Time 1800 sec
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 88.5 %TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 694 Polyester Film
DuPont Teijin Films Melinex® 617 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® 583 Polyester Film, 300 Gauge
DuPont Teijin Films Melinex® 582 Polyester Film, 400 Gauge
DuPont Teijin Films Melinex® 581 Polyester Film

PDTZ9186 / 139528

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.