MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlbond® 1160 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level.

Applications: Pearlbond™ D1160 is used for obtaining PU films by extrusion (blown and cast) for solvent-free adhesion, by heat-seal process.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccISO 2781
Brookfield Viscosity 550 - 1500 cP15% MEK; MQSA 40A
Melt Flow 20 - 60 g/10 min
@Load 21.6 kg,
Temperature 170 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ISO 2781
 
Thermal PropertiesOriginal ValueComments
Melting Point 90.0 - 95.0 °CMQSA 70 A
Softening Point 75.0 - 85.0 °CMQSA 70A
 
Processing PropertiesOriginal ValueComments
Zone 1 115 - 125 °C
Zone 2 165 - 175 °C
Zone 3 175 - 185 °C
Zone 4 165 - 175 °C
Die Temperature 155 - 165 °C
 
Descriptive Properties
Crystallization RateHighMQSA 12 B
Thermoplasticity HighMQSA 68 A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade
Covestro Desmopan® 2590A Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 503 Linear Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 508 Linear Thermoplastic Polyurethane

PMEQU955a / 179135

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.