R50035E is a Linear Low Density Polyethylene grade with balanced density and viscosity designed to provide excellent stress cracking resistance, good mechanical properties with high rigidity, toughness, and low warpage. R50035E is an antioxdant and UV stabilized grade in pellet form.Information provided by SABIC |