MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Premix Thermoplastics PRESEAL® TPE 5011  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: PRESEAL TPE 5011 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket and cable shielding applications. It may also find uses as conductors or in grounding applications. Conductivity is achieved with nickel-coated graphite. PRESEAL TPE 5011 can be extruded like an ordinary thermoplastic elastomer thus giving great new possibilities in mass production. It has adhesion to selected thermoplastics, which opens interesting construction possibilities with co-extrusion e.g. in making combined weather/dust/EMI gaskets. Recyclability is an added value. The material is silicone free.

Typical applications include EMI gaskets in mobile phones, mobile phone base stations and other wireless communication environment as well as in military applications.

* Tension test bar according to ISO 527

Information provided by Premix Thermoplastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.34 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65ISO 7619
Tensile Strength, Ultimate 1.00 MPaISO 37*
Tensile Strength, Yield 1.00 MPaISO 37*
Elongation at Break 330 %ISO 37*
Elongation at Yield 320 %ISO 37*
Modulus of Elasticity 0.00100 GPaISO 178
Compressive Modulus 0.0480 GPaAt 10% Compression; ISO 7743
 0.0490 GPaAt 15% Compression; ISO 7743
 0.0500 GPaAt 18% Compression; ISO 7743
 0.0560 GPaAt 20% Compression; ISO 7743
Tear Strength 8.90 kN/mISO 34-C
Compression Set 50 %
@Temperature 85.0 °C,
Time 86400 sec
ISO 815:1991
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.030 ohm-cmISO Mil-G-835388
Shielding Effectiveness 90 dBISO ARP1705, 20-700 MHz
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 80.0 °CCylinder 1
 150 °CCylinder 2
 180 °CCylinder 3
 200 °CCylinder 4
 200 °CCylinder 5
Adapter Temperature 200 °C
Die Temperature 390 °F
Melt Temperature 195 - 200 °C
Drying Temperature 60.0 °C
@Time 10800 sec
Pre-drying; If stored for longer than 1 year
Moisture Content <= 0.040 %When Produced
Shelf Life 12.0 MonthNormal Storing Conditions
 
Descriptive Properties
AppearanceGranule
ColorGrey

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Premix Thermoplastics PRESEAL® TPE 6071
Premix Thermoplastics PRESEAL® TPE 5010
Premix Thermoplastics PRESEAL 5020 Ni-Coated Graphite
Premix Thermoplastics PRESEAL 6070 Ag-Coated Glass
Premix Thermoplastics PRESEAL 6080 Ag-Coated Glass

PPREMA070 / 58083

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.